by GalGof » Tue Mar 23, 2010 1:43 pm
hm.
founded:
Temperature Quality. The best steel is made by keeping the temperature- the fuel bar- of the crucible/forge at precisely 50%. This means that you can't get good steel by fueling every 7 hours, but instead by fueling every few minutes. For three days.
but i made before 19-21 steel from 23 bars with fueling every 10 hours.. hm.. what q would be if i tried half-fueled o.O