Alloying crucible quality meaningless?

The worst monsters in the Hearthlands warp the fabric of space and time..

Alloying crucible quality meaningless?

Postby Vanigo » Thu Sep 24, 2009 4:38 am

Making bronze, I've noticed that the quality of the alloying crucible and charcoal you use don't seem to affect the quality of the bronze; just the copper and tin quality. Is this intentional?
Vanigo
 
Posts: 146
Joined: Mon Jun 22, 2009 1:03 am

Re: Alloying crucible quality meaningless?

Postby jorb » Thu Sep 24, 2009 4:40 am

Consider it intentional at least for now. We wanted bronze to be relatively simple to make. We might change it.
"The psychological trials of dwellers in the last times will be equal to the physical trials of the martyrs. In order to face these trials we must be living in a different world."

-- Hieromonk Seraphim Rose
User avatar
jorb
 
Posts: 18437
Joined: Fri Apr 03, 2009 7:07 am
Location: Here, there and everywhere.

Re: Alloying crucible quality meaningless?

Postby sonerohi » Fri Sep 25, 2009 2:32 am

Also of note is that it appears to say the result is 1 bronze, but in practice the result is 3. It could just be an issue of it blending in with the rest of the little image though.